Remove oxidation layer and dirt from engine pistons;
Remove burrs from high-precision components such as circuit boards;
Polishing of surgical instruments and implants
Engraving and polishing of high-end glass products and ceramic components;
Clean the plastic mold and make sure the surface is smooth.
Contains no harmful free silicon substances.
High hardness and toughness.
Resistant to high temperature, acid, and alkali, with stable chemical properties.
Recyclable and reusable, good economic benefits.
High density, less dust during sandblasting.
Low cost, high-cost performance.
Wide range of applications, suitable for various metal and non-metal surface treatments.
Brown Fused Aluminum Oxide | ||||
Component | Fe₂O₃ | Al₂O₃ | SiO₂ | TiO₂ |
Numerical Value | 0.3–1.0% | 92.5–97.0% | 1.0–2.0% | 1.5–4.0% |
Color: | Brown | |||
Particle shape: | Angular | |||
Hardness: | Mohs: 9.0 | |||
Specific Gravity: | 3.9–4.0g/cm³ | |||
Bulk density (LPD): | 1.5–2.0g/cm³ |
F Sand | μm | F Sand | μm | F Sand | μm |
F12 | 1400–2000 | F14 | 1180–1700 | F16 | 1000–1400 |
F30 | 500–710 | F36 | 425–600 | F40 | 355–500 |
F70 | 180–250 | F80 | 150–212 | F90 | 125–180 |
F180 | 63–90 | F220 | 53–75 | F24 | 600–850 |
F20 | 850–1180 | F22 | 710–1000 | F60 | 212–300 |
F46 | 300–425 | F54 | 250–355 | F150 | 63–106 |
F100 | 106–150 | F120 | 90–125 |